Description
English: Presented image represents aluminium/nickel coating scratched with diamond indenter. This procedure is called scratch test and is used to analyze adhesion between coating and core material.
English: Presented image represents aluminium/nickel coating scratched with diamond indenter. This procedure is called scratch test and is used to analyze adhesion between coating and core material.
Date
Source Own work
Author hypkulifer

Licensing

[edit]
I, the copyright holder of this work, hereby publish it under the following license:
w:en:Creative Commons
attribution
This file is licensed under the Creative Commons Attribution 4.0 International license.
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.


File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current20:28, 7 December 2021Thumbnail for version as of 20:28, 7 December 20211,439 × 2,560 (1.13 MB)Hypkulifer (talk | contribs)Uploaded own work with UploadWizard

There are no pages that use this file.

Metadata